Customization: | Available |
---|---|
Standard: | JIS, GB, DIN, BS, ASTM, AISI |
Purity: | 78% |
Still deciding? Get samples of US$ 20/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Tankii Resistance Wire 26AWG 32AWG NiCr7030 NiCr8020 Nickel Wire
Product Description
Grade: Ni80Cr20 ,MWS-650,NiCrA,Tophet A,HAI-NiCr 80,Chromel A,Alloy A,N8,Resistohm 80, Stablohm 650,Nichorme V etc.
Resistance wire is a type of wire made from a material with high electrical resistance, such as nichrome.
It is commonly used in heating elements, such as those found in toasters, ovens, and hair dryers, as well as in industrial applications like furnace heating and thermocouples.
The high resistance of the wire allows it to generate heat when an electric current is passed through it, making it an effective heating element.
Parameters of nickel chromium alloy product:
Propertes/Grade | NiCr 80/20 |
NiCr 70/30 |
NiCr 60/15 |
NiCr 35/20 |
NiCr 30/20 |
|
Main Chemical Composition(%) |
Ni |
Bal. |
Bal. |
55.0-61.0 |
34.0-37.0 |
30.0-34.0 |
Cr |
20.0-23.0 |
28.0-31.0 |
15.0-18.0 |
18.0-21.0 |
18.0-21.0 |
|
Fe |
≤ 1.0 |
≤ 1.0 |
Bal. |
Bal. |
Bal. |
|
Max Working Temperature(ºC) |
1200 |
1250 |
1150 |
1100 |
1100 |
|
Resistivity at 20ºC (μ Ω · m) |
1.09 |
1.18 |
1.12 |
1.04 |
1.04 |
|
Density(g/cm3) |
8.4 |
8.1 |
8.2 |
7.9 |
7.9 |
|
Thermal Conductivity (KJ/m· h· ºC) |
60.3 |
45.2 |
45.2 |
43.8 |
43.8 |
|
Coefficient of Thermal Expansion(α × 10-6/ºC) |
18 |
17 |
17 |
19 |
19 |
|
Melting Point(ºC) |
1400 |
1380 |
1390 |
1390 |
1390 |
|
Elongation(%) |
> 20 |
> 20 |
> 20 |
> 20 |
> 20 |
|
Micrographic Structure |
austenite |
austenite |
austenite |
austenite |
austenite |
|
Magnetic Property |
nonmagnetic |
nonmagnetic |
nonmagnetic |
nonmagnetic |
nonmagnetic |
Mechanical Properties of nichrome wire
Max Continuous Service Temperature: |
1250ºC |
Resisivity 20ºC: |
1.18 ohm mm2/m |
Density: |
8.1 g/cm3 |
Thermal Conductivity: |
45.3KJ/m·h·ºC |
Coefficient of Thermal Expansion: |
17 α×10-6/ºC |
Melting Point: |
1380ºC |
Elongation: |
Min 20% |
Micrographic Structure: |
Austenite |
Magnetic Property: |
nonmagnetic |
Temperature Factors Of Electrical Resistivity
20ºC |
100ºC |
200ºC |
300ºC |
400ºC |
500ºC |
600ºC |
1 |
1.006 |
1.012 |
1.018 |
1.025 |
1.026 |
1.018 |
700ºC |
800ºC |
900ºC |
1000ºC |
1100ºC |
1200ºC |
1300ºC |
1.01 |
1.008 |
1.01 |
1.014 |
1.021 |
1.025 |
- |