Resistance Alloy Nichrome Wire NiCr 80/20
Product: Nickel Chromium Wire, nichrome Wire, nichrome flat wire, nichrome ribbon, nichrome tape, nichrome micro wire, NiCrFe Alloy Wire, Chromel Wire
Grade: Nichrome 80/20
Chemical Composition: Nickel 80%, Chrome 20%
Electrical Resistivity: 1.09 ohm mm2/m
Max working temperature: 1200 C
Condition: Bright, Annealed, Soft
Wire diameter 0.015mm-1.0mm packing in spool
Rod, Bar diameter 1mm-30mm
Flat Wire, Ribbon, Foil, Sheet thickness 0.005mm~2.5mm, Width 0.5mm~500mm
Plate: Thickness 2.5mm~7mm, width 10mm~500mm
Producer: Shanghai Tankii Alloy Material Co., Ltd.
We also produce other kinds of nickel chromium alloys, such us NiCr 70/30, NiCr 60/23, NiCr 60/15, NiCr 35/20 and NiCr 30/20.
Chromel A, N8, Nichrome V, HAI-NiCr 80, Tophet A, Resistohm, Ni80Cr20
80, Cronix 80, Protoloy, Alloy A, MWS-650, Stablohm 650, NCHW1
Chromel 70/30, N7, Hytemco, HAI-NiCr 70, Balco, Tophet 30, Ni70Cr30
Resistohm 70, Cronix 70, Stablohm 710
Chromel C, N6, HAI-NiCr 60, Tophet C, Resistohm 60, Cronifer II, Electroloy, Nichrome, Alloy C, MWS-675, Stablohm 675, NCHW2, Ni60Cr15
Chromel D, N4, Chromax, HAI-NiCr 40, Tophet D, Resistohm 40, Cronifer III, 35-20 Ni-Cr, Alloy D, MWS-610, Stablohm 610, Ni35Cr20
Our heating resistance alloys are used to make furnace wire, heating element, resistance element, etching resistor, brake resistor, tube heater, sealor, boile, etc. Because of its high working temperature and high resistivity.
If you have any requirement, pls be free to tell us.
Chemical Composition and Main Properties of Nichrome |
Properties \ Grade |
NiCr 80/20 |
NiCr 70/30 |
NiCr 60/15 |
NiCr 35/20 |
NiCr 30/20 |
Main Chemical Composition |
Ni |
Balance |
Balance |
55.0-61.0 |
34.0-37.0 |
30.0-34.0 |
Cr |
20.0-23.0 |
28.0-31.0 |
15.0-18.0 |
18.0-21.0 |
18.0-21.0 |
Fe |
≤1.0 |
≤1.0 |
Balance |
Balance |
Balance |
Max Continuous Service Temperature(C) |
1200 |
1250 |
1150 |
1100 |
1100 |
Resisivity 20oC (Ωmm2/m) |
1.09 |
1.18 |
1.12 |
1.04 |
1.04 |
Density (g/cm3) |
8.4 |
8.1 |
8.2 |
7.9 |
7.9 |
Thermal Conductivity(KJ/m@h@oC) |
60.3 |
45.2 |
45.2 |
43.8 |
43.8 |
Coefficient of Thermal Expansion(α×10-6/oC) |
18 |
17 |
17 |
19 |
19 |
Melting Point( C) |
1400 |
1380 |
1390 |
1390 |
1390 |
Elongation(%) |
>20 |
>20 |
>20 |
>20 |
>20 |
Micrographic Structure |
austenite |
austenite |
austenite |
austenite |
austenite |
Magnetic Property |
nonmagnetic |
nonmagnetic |
nonmagnetic |
Weak magnetic |
Weak magnetic |