nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil

Product Details
Customization: Available
Product Type: Wire
Material: Ni-Fe Alloy
Manufacturer/Factory, Trading Company

360° Virtual Tour

Diamond Member Since 2008

Suppliers with verified business licenses

Audited Supplier

Audited by an independent third-party inspection agency

Plant Area
>2000 square meters
Export Year
2008-08-20
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
  • nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
Find Similar Products

Basic Info.

Model NO.
1J79
Carbon Content
Low Carbon
PCD
98mm
ET
35mm
Hole
4
Diameter
0.1~25mm
Transport Package
Coil, Pallet, Wooden Case
Specification
RoHS
Trademark
SMTK 79-W
Origin
China
HS Code
750522000
Production Capacity
3000 Tons/Year

Product Description

 Nickel-iron Magnetic Alloy Ni79Mo4, E11c, Permalloy, 79HM 1J79 Alloy Foil

Classification: precision soft magnetic alloy
Supplement: Alloy with high permeability in weak fields at saturation induction 0.65-0.75 T. Alloy 1J79/ permally high squareness of the hysteresis loop and a low coefficient of magnetization reversal
Application: For small cores of transformers, chokes and relays operating in weak fields, magnetic shields. In the small thickness (0.05 ± 0.02 mm) - cores for pulse transformers, magnetic amplifiers and solid state relays

Chemical composition
composition C P S Mn Si
Content(%) 0.03 0.02 0.02 0.6~1.1 0.3~0.5
 
composition Ni Cr Mo Cu Fe
Content(%) 78.5~80.0 - 3.8~4.1 ≤0.2 Bal
Heat treatment system
shop sign Annealing medium heating temperature Keep the temperature time/h Cooling rate

1j79
Dry hydrogen or vacuum, pressure is not greater than 0.1 Pa Along with the furnace heating up 1100~1150ºC
3~6
In 100 ~ 200 ºC / h speed cooling to 600 ºC, fast to 300 ºC draw a charge

nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil
nickel–iron magnetic alloy Ni79Mo4, E11c, malloy, permalloy, 79HM 1J79 alloy foil

 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now
Contact Supplier