Customization: | Available |
---|---|
Standard: | GB |
Purity: | - |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Alloy | Ni% | Mn% | Fe% | Si% | Cu% | C% | S% |
Nickel 200 | Min 99.2 | Max 0.35 | Max 0.4 | Max 0.35 | Max 0.25 | Max 0.15 | Max 0.01 |
Density | 8.89g/cm3 |
Specific Heat | 0.109(456 J/kg.ºC) |
Electrical Resistivity | 0.096×10-6ohm.m |
Melting Point | 1435-1446ºC |
Thermal Conductivity | 70.2 W/m-K |
Mean Coeff Thermal Expansion | 13.3×10-6m/m.ºC |
Mechanical Properties | Nickel 200 |
Tensile Strength | 462 Mpa |
Yield Strength | 148 Mpa |
Elongation | 47% |
Bar | Forging | Pipe | Sheet/Strip | Wire | |
ASTM | ASTM B160 | ASTM B564 | ASTM B161/B163/B725/B751 | AMS B162 | ASTM B166 |
Main Composition % | |||
Ni | Mn | Si | |
NiMn2 | Bal. | 1.5-2.5 | 0.3 |
NiMn3 | Bal. | 2.3-3.3 | 0.3 |
NiMn5 | Bal. | 4.6-5.4 | 0.5 |
Code No. | Dia. mm | TS. N/mm2 | Elongation % |
NiMn2 | ≤6.0 | ≥350 | ≥20 |
NiMn3 | ≤6.0 | ≥350 | ≥20 |
NiMn5 | ≤6.0 | ≥350 | ≥20 |