Customization: | Available |
---|---|
Product Type: | Wire |
Material: | CuNi |
Still deciding? Get samples of US$ 30/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Product Description
These enameled resistance wires have been broadly used for standard resistors, automobile
parts, winding resistors, etc. using the insulation processing best suited for these applications, taking full advantage of the distinctive features of enamel coating.
Type Of Bare Alloy Wire
The alloy we can do enamelled are Copper-nickel alloy wire,Constantan wire,Manganin wire. Kama Wire,NiCr Alloy wire,FeCrAl Alloy wire etc alloy wire
Size:
Round wire:0.018mm~3.0mm
Color of enamel insulation:Red,Green,Yellow,Black,Blue,Nature etc.
Ribbon Size:0.01mm*0.2mm~1.2mm*24mm
Moq:5kg each size
nicr8020 alloy heating wire
1.About Nichrome wire
Nichrome alloy includes pure nickel, NiCr alloy, Fe-Cr-Al alloy and copper nickel alloy.
Nickel chrome alloys: Ni80Cr20, Ni70Cr30, Ni60Cr15, Ni35Cr20, Ni30Cr20, Cr25Ni20, pure nickel Ni200 and Ni201
FeCrAl alloy: 0Cr25Al5, 0Cr23Al5, 0Cr21Al4, 0Cr27Al7Mo2, 0Cr21Al6Nb, 0Cr21Al6.
Copper nickel alloy: CuNi1, CuNi2, CuNi6, CuNi8, CuNi10, CuNi23, CuNi30, CuNi44, Constantan,CuMn12Ni
Our Nichrome alloy are in the form of wire, coil, ribbon, strip, foil
size:Wire: 0.01mm-10mm Ribbon: 0.05*0.2mm-2.0*6.0mm Strip: 0.5*5.0mm-5.0*600mm Bar: 10-100mm
Insulation-enamelled Name |
Thermal LevelºC (working time 2000h) |
Code Name |
GB Code |
ANSI. TYPE |
Polyurethane enamelled wire |
130 |
UEW |
QA |
MW75C |
Polyester enamelled wire |
155 |
PEW |
QZ |
MW5C |
Polyester-imide enamelled wire |
180 |
EIW |
QZY |
MW30C |
Polyester-imide and polyamide-imide double coated enameled wire |
200 |
EIWH (DFWF) |
QZY/XY |
MW35C |
Polyamide-imide enamelled wire |
220 |
AIW |
QXY |
MW81C |
1) Polyester resistance wire , class 130
2) Modified polyester resistance wire , class 155
3) Polyesterimide resistance wire , class 180
4) Polyester (imide) coated with polyamide-imide resistance wire , class 200
5) Polyimide resistance wire , class 220
Tpye of Bare Wire
main property type |
|
Cuni1 |
CuNI2 |
CuNI6 |
CuNi8 |
CuNI10 |
CuNi14 |
CuNi19 |
CuNi23 |
CuNi30 |
CuNi34 |
CuNI44 |
|
main chemical composition |
Ni |
1 |
2 |
6 |
8 |
10 |
14.2 |
19 |
23 |
30 |
34 |
44 |
|
|
MN |
/ |
/ |
/ |
/ |
/ |
0.3 |
0.5 |
0.5 |
1.0 |
1.0 |
1.0 |
|
|
CU |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
rest |
|
max working temperature |
|
/ |
200 |
220 |
250 |
250 |
300 |
300 |
300 |
350 |
350 |
400 |
|
density g/cm3 |
|
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
8.9 |
|
resistivity at 20 °c |
|
0.03 ± 10% |
0.05± 10% |
0.10± 10% |
0.12± 10% |
0.15± 10% |
0.20± 5% |
0.25± 5% |
0.30± 5% |
0.35± 5% |
0.40± 5% |
0.49± 5% |
|
temperature coefficient of resistance |
|
<100 |
<120 |
<60 |
<57 |
<50 |
<38 |
<25 |
<16 |
<10 |
-0 |
<-6 |
|
tensile strength mpa |
|
>210 |
>220 |
>250 |
>270 |
>290 |
>310 |
>340 |
>350 |
>400 |
>400 |
>420 |
|
elongation |
|
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
>25 |
|
melting point °c |
|
1085 |
1090 |
1095 |
1097 |
1100 |
1115 |
1135 |
1150 |
1170 |
1180 |
1280 |
|
coefficient of conductivity |
|
145 |
130 |
92 |
75 |
59 |
48 |
38 |
33 |
27 |
25 |
23 |