Customization: | Available |
---|---|
Type: | Copper Wire |
Application: | Air Condition or Refrigerator, Water Tube, Water Heater, Oil Cooler Pipe |
Still deciding? Get samples of US$ 22/kg
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Ni | Mn | Fe | Si | Cu | Other | ROHS Directive | |||
Cd | Pb | Hg | Cr | ||||||
2 | - | - | - | Bal | - | ND | ND | ND | ND |
Max Continuous Service Temp | 200ºC |
Resisivity at 20ºC | 0.05±10%ohm mm2/m |
Density | 8.9 g/cm3 |
Thermal Conductivity | 100(max) |
Melting Point | 1280ºC |
Tensile Strength,N/mm2 Annealed,Soft | 140~310 Mpa |
Tensile Strength,N/mm2 Cold Rolled | 280~620 Mpa |
Elongation(anneal) | 25%(min) |
Elongation(cold rolled) | 2%(min) |
EMF vs Cu, μV/ºC (0~100ºC) | -8 |
Micrographic Structure | austenite |
Magnetic Property | Non |
Chemical Composition and Main Property of Cu-Ni Low Resistance Alloy | ||||||||
PropertiesGrade | CuNi1 | CuNi2 | CuNi6 | CuNi8 | CuMn3 | CuNi10 | ||
Main Chemical Composition | Ni | 1 | 2 | 6 | 8 | _ | 10 | |
Mn | _ | _ | _ | _ | 3 | _ | ||
Cu | Bal | Bal | Bal | Bal | Bal | Bal | ||
Max Continuous Service Temperature(º C) | 200 | 200 | 200 | 250 | 200 | 250 | ||
Resisivity at 2º C (Ω mm2/m) | 0.03 | 0.05 | 0.1 | 0.12 | 0.12 | 0.15 | ||
Density(g/cm3) | 8.9 | 8.9 | 8.9 | 8.9 | 8.8 | 8.9 | ||
Thermal Conductivity(α × 10-6º C) | < 100 | < 120 | < 60 | < 57 | < 38 | < 50 | ||
Tensile Strength(Mpa) | ≥ 210 | ≥ 220 | ≥ 250 | ≥ 270 | ≥ 290 | ≥ 290 | ||
EMF vs Cu(μ Vº C)(0~10º C) | -8 | -12 | -12 | -22 | _ | -25 | ||
Approximate Melting Point(º C) | 1085 | 1090 | 1095 | 1097 | 1050 | 1100 | ||
Micrographic Structure | austenite | austenite | austenite | austenite | austenite | austenite | ||
Magnetic Property | non | non | non | non | non | non | ||
PropertiesGrade | CuNi14 | CuNi19 | CuNi23 | CuNi30 | CuNi34 | CuNi44 | ||
Main Chemical Composition | Ni | 14 | 19 | 23 | 30 | 34 | 44 | |
Mn | 0.3 | 0.5 | 0.5 | 1 | 1 | 1 | ||
Cu | Bal | Bal | Bal | Bal | Bal | Bal | ||
Max Continuous Service Temperatureº C) | 300 | 300 | 300 | 350 | 350 | 400 | ||
Resisivity at 2º C (Ω mm2/m) | 0.2 | 0.25 | 0.3 | 0.35 | 0.4 | 0.49 | ||
Density(g/cm3) | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | 8.9 | ||
Thermal Conductivity(α × 10-6º C) | < 30 | < 25 | < 16 | < 10 | < 0 | < -6 | ||
Tensile Strength(Mpa) | ≥ 310 | ≥ 340 | ≥ 350 | ≥ 400 | ≥ 400 | ≥ 420 | ||
EMF vs Cu(μ Vº C)(0~10º C) | -28 | -32 | -34 | -37 | -39 | -43 | ||
Approximate Melting Point(º C) | 1115 | 1135 | 1150 | 1170 | 1180 | 1280 | ||
Micrographic Structure | austenite | austenite | austenite | austenite | austenite | austenite | ||
Magnetic Property | non | non | non | non | non | non |